Maintenance of die-casting material cylinder, punch, and soup supply, control of punch jamming, gas entrapment, and punch wear
The material cylinder (pressure chamber) and punch are the inlet of the injection system, and many air holes, cold materials, and coil air sources are not in the mold, but in the pressure chamber and punch.
1、 Punch material and coating
Ductile iron punch has high cost-effectiveness; H13 punch is suitable for long-term mass production at high temperatures; AlTiN or specialized high-temperature lubricating coating on the surface of the punch; The gap between the punch and the barrel is 0.08-0.15mm, and the gap is large due to aluminum and rolled air; The gap is small and it gets stuck due to heat.
2、 Punch lubrication
Graphite lubrication, oil-based lubrication; Excessive lubrication can decompose and produce gas, causing porosity in castings; Insufficient lubrication, wear and jamming of the punch; Quantitative oil feeding devices are commonly used in foreign trade automation machines.
3、 Filling rate of material cylinder
The proportion of the volume of aluminum liquid loaded into the barrel to the volume of the barrel; The filling rate is too low, and there is a large amount of air in the upper part of the material cylinder, which is prone to air entrapment during the slow injection stage; The conventional filling rate is 70-85%.
4、 Slow injection and barrel coordination
Slow injection speed control 0.1-0.4m/s, smoothly push the aluminum liquid into the sprue, and discharge the air inside the barrel from the sprue and overflow; Slow injection is too fast, causing the aluminum liquid to roll and curl.
5、 Common faults
Punch wear → increased clearance, aluminum running, unstable injection; Overheating and insufficient lubrication of the punch → locking; Aluminum nodules on the inner wall of the barrel → scratching the punch and introducing impurities; Fluctuations in barrel temperature → premature solidification of aluminum liquid.
6、 Maintenance cycle
Regularly measure the outer diameter of the punch and replace it if the wear exceeds the standard; Regularly clean the aluminum deposits in the material barrel; The temperature control of the material cylinder is stable, avoiding severe fluctuations in temperature. Google's "die casting shot sleeve and plunger maintenance" is aimed at device engineers.
FAQ
Is it better to have a higher filling rate?
Too high, no buffer space, aluminum liquid is prone to splashing out from the barrel mouth.
2. What if the punch sticks and pulls hard?
Pulling the inner wall of the material cylinder, the material cylinder is scrapped, and the cost is very high.
What is the defect of excessive graphite lubrication?
Carbon gas, mixed with pores and black spots.
4. Should the material barrel be heated?
Preheat the material cylinder to prevent the aluminum liquid from instantly skinning the cold material when it comes into contact with the cold cylinder.
What is the reason for unilateral wear of the punch clearance?
Poor guidance of the punch and misalignment of the material cylinder.
Is the slow injection speed a fixed value?
Adjust with filling rate, alloy, and barrel diameter.
How to clean aluminum nodules on the material barrel?
Scrape off after cooling down, and do not forcefully knock or damage the inner wall.
8. Is there a material cylinder punch for low-pressure casting?
No, the low pressure relies on the liquid lifting tube, and the entire feeding logic is completely different.
Формы для литья под низким давлением (LPDC)
Формы для гравитационного литья
Формы для литья под противодавлением (CPC)
Формы для литья конструкционных деталей
Форма для литья ступицы колеса мотоцикла
Форма для литья ступицы колеса под дифференциальным давлением
Форма для гравитационного литья ступицы колеса
Форма для литья ступицы колеса под низким давлением
ФОРМЫ ДЛЯ АВТОМОБИЛЬНЫХ КОЛЕС
КОНСТРУКЦИОННЫЕ ДЕТАЛИ ДЛЯ АВТОМОБИЛЕЙ
ДРУГИЕ АЛЮМИНИЕВЫЕ ЛИТНЫЕ ДЕТАЛИ
ПРОФИЛЬ КОМПАНИИ
ОРГАНИЗАЦИОННАЯ СТРУКТУРА
ИСТОРИЯ РАЗВИТИЯ
ИНТЕЛЛЕКТУАЛЬНАЯ СОБСТВЕННОСТЬ
КОМАНДНЫЙ ДУХ И ПАРТНЕРЫ
Авторские права © Zhejiang Xinfeng Machinery Co., Ltd. Все права защищены.